Mechanical Behavior of PLA Based Composite Filaments Fabricated by FDM: Role of Build Orientation and Reinforcement Type


Cokyasar M. E., ÖZMEN U.

JOURNAL OF APPLIED POLYMER SCIENCE, cilt.143, sa.38, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 143 Sayı: 38
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1002/app.71205
  • Dergi Adı: JOURNAL OF APPLIED POLYMER SCIENCE
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Aerospace Database, Applied Science & Technology Source, Chemical Abstracts Core, Chimica, Compendex, INSPEC, Materials Science & Engineering Collection (ProQuest), Technology Collection (ProQuest)
  • Anahtar Kelimeler: build orientation, carbon fiber, ceramic, FDM, foaming agent, polylactic acid, wood
  • Manisa Celal Bayar Üniversitesi Adresli: Evet

Özet

This research highlights the necessity of concurrently evaluating filament type and printing orientation to optimize the balance between stiffness and ductility. Mechanical properties of polylactic acid (PLA) based composite filaments (neat, carbon fiber (CF), wood, ceramic, and foaming agent (FA)) manufactured via Fused deposition modeling (FDM) were experimentally investigated. Specimens were fabricated at 0 degrees, 30 degrees, 45 degrees, 60 degrees, and 90 degrees build orientations and tested according to ASTM (D638 (Tensile), D790 (Three point bending), D6110 (Charpy), and D2240 (Shore D)) standards. Results demonstrated that mechanical performance is significantly influenced by material composition and build orientation. Tensile testing revealed that 60 degrees oriented CF reinforced specimens exhibited the highest elastic modulus (4.31 GPa), whereas PLA FA at 60 degrees yielded the lowest (0.87 GPa). In three point bending, 0 degrees Neat PLA achieved the maximum flexural strength (74.48 MPa), while 60 degrees PLA FA recorded the minimum (35.32 MPa). Charpy impact analyses indicated maximum toughness in 0 degrees Wood specimens (19.18 kJ/m2) and the lowest at 60 degrees orientation (2.11 kJ/m2). Furthermore, 45 degrees Ceramic reinforced specimens attained a maximum surface hardness of 57 HD, contrasting with the minimum 15 HD in 0 degrees PLA FA. The 90 degrees build orientation significantly reduced mechanical strength across material groups due to poor interlayer adhesion.