SIMULATION-BASED STUDY ON THERMOMECHANICAL RESPONSE OF DP600 STEEL UNDER LASER WELDING CONDITIONS


Creative Commons License

Küçükdoğan Öztürk N., Orta H. T.

6.Palestra Congress, Skopje, Makedonya, 27 - 30 Temmuz 2025, cilt.1, ss.213-223, (Tam Metin Bildiri)

  • Yayın Türü: Bildiri / Tam Metin Bildiri
  • Cilt numarası: 1
  • Doi Numarası: 10.30546/19023.978-9952-8589-3-8.2025.0016
  • Basıldığı Şehir: Skopje
  • Basıldığı Ülke: Makedonya
  • Sayfa Sayıları: ss.213-223
  • Manisa Celal Bayar Üniversitesi Adresli: Evet

Özet

Thermomechanical simulations of DP600 high-strength steel under laser welding conditions were conducted using Simufact Welding software to assess the process’s reliability and consistency. Four

separate analyses yielded consistent displacement values in the X, Y, and Z directions, with the

highest displacement observed along the Z-axis (0.12 mm), indicating minimal thermal distortion. The

total displacement remained constant at 0.76 mm, reflecting uniform thermal expansion and

contraction during welding. Plastic strain and elastic strain values were minimal and stable across simulations, at 0.004% and 0.001%, respectively, demonstrating limited permanent deformation and effective elastic recovery. Equivalent stresses ranged moderately between 219.48 MPa and 247.36

MPa, with the highest normal stresses in the X direction, followed by Y and Z directions.Thermal analyses, supported by four temperature distribution snapshots (Figures a–d), revealed localized heating with Gaussian-like profiles centered on the weld line. Maximum temperatures ranged between approximately 939°C and 964°C, consistent with DP600’s melting range and confirming sufficient energy input for proper fusion. The heat-affected zone (HAZ) exhibited symmetrical distribution and

gradual thermal gradients, aligning with low thermal distortion findings. Increasing welding speed

reduced peak temperatures while broadening the thermal profile, indicating a trade-off between heat

input and HAZ extent.A three-dimensional temperature distribution model further illustrated the

temperature variation across the weld distance and welding speeds. At lower welding speeds (~1.6 mm/s), peak temperatures approached 950°C, ensuring sufficient energy input for effective fusion. Increasing the welding speed to ~2.2 mm/s resulted in a gradual decline in peak temperature and a broader but cooler HAZ. This controlled thermal gradient is crucial for balancing weld quality,

mechanical integrity, and dimensional accuracy by preventing abrupt phase changes or stress

concentrations.