Mechanical characterization of mussel shell powder-filled glass fibre/epoxy composites: effect of content, calcination and seawater aging


Okkalı E. B., TAŞ H.

Journal of the Brazilian Society of Mechanical Sciences and Engineering, cilt.48, sa.15, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 48 Sayı: 15
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1007/s40430-026-07012-2
  • Dergi Adı: Journal of the Brazilian Society of Mechanical Sciences and Engineering
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Aerospace Database, Compendex, INSPEC, Materials Science & Engineering Collection (ProQuest), Technology Collection (ProQuest)
  • Anahtar Kelimeler: Aging, Calcination, Mechanical characterization, Mechanical properties, Mussel shell, Water uptake
  • Manisa Celal Bayar Üniversitesi Adresli: Evet

Özet

This study investigated the use of mussel shell (MS) powder as a bio-filler in glass fibre-reinforced epoxy composites. Glass fibre/epoxy composites incorporating 0 wt.%, 5 wt.%, 10 wt.%, and 15 wt.% non-calcined MS (C-MS) powder, as well as 5 wt.% calcined MS (C+MS) powder, were fabricated using the hand lay-up method. Tensile, three-point bending, and low-velocity impact tests were conducted. Furthermore, seawater aging tests were performed in artificial seawater (3.5 wt.% NaCl) at 25 °C for 78 days to evaluate water uptake behaviour and durability performance. Results showed that incorporation of 5 wt.% C-MS powder significantly improved the mechanical performance of the composites. Tensile strength and Young’s modulus increased by 10.2% and 4.1%, respectively, while flexural strength and flexural modulus improved by 6.8% and 6.0%, respectively. In low-velocity impact tests, the addition of 5 wt.% C-MS powder increased the maximum contact force by 18.6% and reduced absorbed energy by 20.3%. However, increasing the filler content to 10 wt.% and 15 wt.% reduced tensile and flexural properties due to particle agglomeration and stress concentration. The calcination process adversely affected both the mechanical and aging performance of the composites. The composite containing 5 wt.% C+MS powder exhibited 71.6% higher water absorption than the unfilled composite after 78 days of aging and showed significant reductions in tensile strength and stiffness. Overall, the study demonstrated that C-MS powder can be effectively utilized as a sustainable and environmentally friendly bio-filler for improving the performance of glass fibre/epoxy composites, particularly at low filler contents.