Quasi-static indentation behavior of glass fiber reinforced sandwich composites with asymmetric facesheets and segmented polymer foam cores


YALKIN H. E.

Journal of the Brazilian Society of Mechanical Sciences and Engineering, cilt.48, sa.14, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 48 Sayı: 14
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1007/s40430-026-06948-9
  • Dergi Adı: Journal of the Brazilian Society of Mechanical Sciences and Engineering
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Aerospace Database, Compendex, INSPEC, Materials Science & Engineering Collection (ProQuest), Technology Collection (ProQuest)
  • Anahtar Kelimeler: Damage tolerance, E-glass fiber, Energy absorption, Indenter geometry, PVC foam, Quasi-static indentation, Sandwich composites
  • Manisa Celal Bayar Üniversitesi Adresli: Evet

Özet

This study examines the quasi-static indentation response of E-glass fiber-reinforced epoxy/PVC foam sandwich composites with different through-thickness structures. Although foam-core sandwich panels, multilayered cores, asymmetric facesheets, and indenter-shape effects have been studied separately, systematic data obtained by combining these parameters within a single material system and test configuration are still limited. The contribution of this work is therefore a controlled comparison of facesheet asymmetry, foam-core segmentation, and indenter geometry in one experimental matrix. Six configurations were manufactured by vacuum assisted resin infusion: a monolithic laminate (L), a symmetric sandwich panel (3C3), two asymmetric single-core panels (5C1 and 4C2), and two double-core panels (2c2c2 and 4c1c1). The specimens were tested using three indenter geometries, namely a 12.7 mm hemispherical indenter (H12.7), a 6.35 mm hemispherical indenter (H6.35), and a 12.7 mm diameter 45° conical indenter (C45), with three repetitions for each combination. A separate two-way analysis of variance showed significant effects of specimen configuration, indenter geometry, and their interaction on peak force, absorbed energy, and indentation stiffness (all p < 0.001). Peak force, absorbed energy, and indentation stiffness were evaluated from the load–displacement curves and reported as mean standard deviation. The results show that indenter geometry and structure jointly controlled the indentation response. The highest peak force and absorbed energy were obtained for the 2c2c2 configuration under C45 loading, reaching 9174.0 N and 97.5 J, respectively. In contrast, the monolithic laminate exhibited the greatest initial stiffness, with a maximum value of 1285.8 N/mm under H12.7 loading. The smaller hemispherical indenter generally produced lower absorbed energy, especially in the sandwich configurations, whereas the conical indenter promoted progressive penetration and higher energy dissipation in the double-core panels. Within the tested range, the double-core architecture absorbed up to 67.2% more energy than the symmetric single-core panel even though its initial indentation stiffness was lower. This finding provides a clearer design rationale for damage-tolerant sandwich panels in which progressive crushing and internal load redistribution are proposed mechanisms for improving energy absorption relative to stiffness alone.