Effect of Fe2O3 and FeOOH dopants on the optical and mechanical properties of 4Y-TZP dental ceramics


Ergani E. S., YALAMAÇ E., SÜTÇÜ M.

Ceramics International, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1016/j.ceramint.2026.10.472
  • Dergi Adı: Ceramics International
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Chemical Abstracts Core, Compendex, INSPEC, Academic Search Ultimate (EBSCO), Engineering Source (EBSCO)
  • Anahtar Kelimeler: Dental ceramics, Iron-based dopants, Mechanical properties, Opacity, Zirconia
  • Manisa Celal Bayar Üniversitesi Adresli: Evet

Özet

The effects of Fe2O3 and FeOOH additives (0.40 and 0.60 wt%) on the optical, thermal, structural, mechanical and microstructural properties of 4 mol% yttria-stabilized zirconia (4Y-TZP) ceramics were investigated. Optical properties were evaluated using CIE Lab* coordinates, opacity and color differences (ΔE00) relative to a commercial pre-colored reference. Phase composition was assessed by X-ray diffraction and Rietveld refinement. Grain morphology and size were characterized by SEM. Mechanical performance was examined through biaxial flexural strength (BFS), Vickers hardness and indentation fracture resistance tests. Weibull analysis assessed BFS strength variability. Fe-containing compositions exhibited red–yellow color shifts and high opacity (98.45–99.99%). One-way ANOVA identified significant differences in L*, a* and b* among Fe-containing compositions (all p < 0.001), but not in opacity (p = 0.247). At the nominal 0.60 wt% addition level, 4Y-60FH showed closer color similarity to the commercial reference (ΔE00 = 1.63) than 4Y-60F (3.26). The tetragonal phase remained dominant in the four examined compositions with phase fractions ranging from 83.6% to 89.3%.FeOOH containing compositions exhibited finer grains than their Fe2O3 containing counterparts; mean grain sizes were 550 and 634 nm for 4Y-60FH and 4Y-60F, respectively. Fe-containing compositions showed lower mean BFS (638.47–665.57 MPa) than undoped 4Y (725.55 MPa), with reduced Vickers hardness. Nevertheless, 4Y-60FH exhibited a higher Weibull modulus than 4Y-60F (35.10 versus 19.32) and the highest numerical indentation fracture resistance (3.60 MPa m1/2). These findings support FeOOH as a potential alternative coloring precursor, particularly at 0.60 wt% nominal addition, although precursor chemistry and Fe2O3-equivalent concentration effects cannot be fully separated.